In galvanic corrosion, which component tends to be protected from corrosion?

Prepare for the Navy Parachute Rigger Test. Utilize flashcards and sewing-related questions with detailed explanations. Ensure your exam success!

Multiple Choice

In galvanic corrosion, which component tends to be protected from corrosion?

Explanation:
In galvanic corrosion, when two metals are in electrical contact in an electrolyte, electrons flow from the more active metal to the more noble metal. The active metal becomes the anode and corrodes, while the noble metal acts as the cathode and is protected from corrosion. So the component that tends to be protected is the cathode. The anode would be the one that corrodes, and uniform surface corrosion or pitting describe patterns of damage rather than a protected component.

In galvanic corrosion, when two metals are in electrical contact in an electrolyte, electrons flow from the more active metal to the more noble metal. The active metal becomes the anode and corrodes, while the noble metal acts as the cathode and is protected from corrosion. So the component that tends to be protected is the cathode. The anode would be the one that corrodes, and uniform surface corrosion or pitting describe patterns of damage rather than a protected component.

Subscribe

Get the latest from Examzify

You can unsubscribe at any time. Read our privacy policy